Changes in the tailing properties (increasing clay mineral content and fine particles) and poor operation of the dewatering systems have negative impacts on the Tailing Storage Facilities (TSF) of the Shahrbabak copper complex. The design solid concentration of the thickened tailings is 63 wt.% in the Shahrbabak paste plant but it is well below the …